Crystallography Open Database
Search results
Result: there are 63 entries in the selection
Switch to the old layout of the pageDownload all results as: list of COD numbers | list of CIF URLs | data in CSV format | archive of CIF files (ZIP)
Searching journal of publication like 'Physics and Chemistry of Minerals' volume of publication is 17
COD ID | Links | Formula | Space group | Cell parameters | Cell volume | Bibliography |
---|---|---|---|---|---|---|
9005883 | CIF | Al O3 Sc | P b n m | 4.937; 5.2321; 7.2045 90; 90; 90 | 186.099 | Hill, R. J.; Jackson, I. The thermal expansion of ScAlO3 - a silicate perovskite analogue Sample: T = 10 C Physics and Chemistry of Minerals, 1990, 17, 89-96 |
9005884 | CIF | Al O3 Sc | P b n m | 4.9597; 5.2471; 7.2353 90; 90; 90 | 188.292 | Hill, R. J.; Jackson, I. The thermal expansion of ScAlO3 - a silicate perovskite analogue Sample: T = 500 C Physics and Chemistry of Minerals, 1990, 17, 89-96 |
9005885 | CIF | Al O3 Sc | P b n m | 4.9767; 5.2584; 7.2604 90; 90; 90 | 190.001 | Hill, R. J.; Jackson, I. The thermal expansion of ScAlO3 - a silicate perovskite analogue Sample: T = 800 C Physics and Chemistry of Minerals, 1990, 17, 89-96 |
9005886 | CIF | Al O3 Sc | P b n m | 4.993; 5.269; 7.2846 90; 90; 90 | 191.644 | Hill, R. J.; Jackson, I. The thermal expansion of ScAlO3 - a silicate perovskite analogue Sample: T = 1100 C Physics and Chemistry of Minerals, 1990, 17, 89-96 |
9005887 | CIF | Co3 O4 | F d -3 m :2 | 8.0821; 8.0821; 8.0821 90; 90; 90 | 527.926 | Liu, X.; Prewitt, C. T. High-temperature X-ray diffraction study of Co3O4: transition from normal to disordered spinel Sample: RUN I, T = 301 K Physics and Chemistry of Minerals, 1990, 17, 168-172 |
9005888 | CIF | Co3 O4 | F d -3 m :2 | 8.0968; 8.0968; 8.0968 90; 90; 90 | 530.811 | Liu, X.; Prewitt, C. T. High-temperature X-ray diffraction study of Co3O4: transition from normal to disordered spinel Sample: RUN I, T = 580 K Physics and Chemistry of Minerals, 1990, 17, 168-172 |
9005889 | CIF | Co3 O4 | F d -3 m :2 | 8.1178; 8.1178; 8.1178 90; 90; 90 | 534.952 | Liu, X.; Prewitt, C. T. High-temperature X-ray diffraction study of Co3O4: transition from normal to disordered spinel Sample: RUN I, T = 892 K Physics and Chemistry of Minerals, 1990, 17, 168-172 |
9005890 | CIF | Co3 O4 | F d -3 m :2 | 8.1289; 8.1289; 8.1289 90; 90; 90 | 537.15 | Liu, X.; Prewitt, C. T. High-temperature X-ray diffraction study of Co3O4: transition from normal to disordered spinel Sample: RUN I, T = 995 K Physics and Chemistry of Minerals, 1990, 17, 168-172 |
9005891 | CIF | Co3 O4 | F d -3 m :2 | 8.1484; 8.1484; 8.1484 90; 90; 90 | 541.025 | Liu, X.; Prewitt, C. T. High-temperature X-ray diffraction study of Co3O4: transition from normal to disordered spinel Sample: RUN I, T = 1098 K Physics and Chemistry of Minerals, 1990, 17, 168-172 |
9005892 | CIF | Co3 O4 | F d -3 m :2 | 8.1637; 8.1637; 8.1637 90; 90; 90 | 544.078 | Liu, X.; Prewitt, C. T. High-temperature X-ray diffraction study of Co3O4: transition from normal to disordered spinel Sample: RUN I, T = 1144 K Physics and Chemistry of Minerals, 1990, 17, 168-172 |
9005893 | CIF | Co3 O4 | F d -3 m :2 | 8.1773; 8.1773; 8.1773 90; 90; 90 | 546.802 | Liu, X.; Prewitt, C. T. High-temperature X-ray diffraction study of Co3O4: transition from normal to disordered spinel Sample: RUN I, T = 1170 K Physics and Chemistry of Minerals, 1990, 17, 168-172 |
9005894 | CIF | Co3 O4 | F d -3 m :2 | 8.1893; 8.1893; 8.1893 90; 90; 90 | 549.212 | Liu, X.; Prewitt, C. T. High-temperature X-ray diffraction study of Co3O4: transition from normal to disordered spinel Sample: RUN I, T = 1185 K Physics and Chemistry of Minerals, 1990, 17, 168-172 |
9005895 | CIF | Co3 O4 | F d -3 m :2 | 8.1975; 8.1975; 8.1975 90; 90; 90 | 550.864 | Liu, X.; Prewitt, C. T. High-temperature X-ray diffraction study of Co3O4: transition from normal to disordered spinel Sample: RUN I, T = 1201 K Physics and Chemistry of Minerals, 1990, 17, 168-172 |
9005896 | CIF | Co3 O4 | F d -3 m :2 | 8.0837; 8.0837; 8.0837 90; 90; 90 | 528.239 | Liu, X.; Prewitt, C. T. High-temperature X-ray diffraction study of Co3O4: transition from normal to disordered spinel Sample: RUN II, T = 296 K Physics and Chemistry of Minerals, 1990, 17, 168-172 |
9005897 | CIF | Co3 O4 | F d -3 m :2 | 8.1099; 8.1099; 8.1099 90; 90; 90 | 533.392 | Liu, X.; Prewitt, C. T. High-temperature X-ray diffraction study of Co3O4: transition from normal to disordered spinel Sample: RUN II, T = 773 K Physics and Chemistry of Minerals, 1990, 17, 168-172 |
9005898 | CIF | Co3 O4 | F d -3 m :2 | 8.1439; 8.1439; 8.1439 90; 90; 90 | 540.129 | Liu, X.; Prewitt, C. T. High-temperature X-ray diffraction study of Co3O4: transition from normal to disordered spinel Sample: RUN II, T = 1073 K Physics and Chemistry of Minerals, 1990, 17, 168-172 |
9005899 | CIF | Co3 O4 | F d -3 m :2 | 8.1546; 8.1546; 8.1546 90; 90; 90 | 542.261 | Liu, X.; Prewitt, C. T. High-temperature X-ray diffraction study of Co3O4: transition from normal to disordered spinel Sample: RUN II, T = 1123 K Physics and Chemistry of Minerals, 1990, 17, 168-172 |
9005900 | CIF | Co3 O4 | F d -3 m :2 | 8.1691; 8.1691; 8.1691 90; 90; 90 | 545.158 | Liu, X.; Prewitt, C. T. High-temperature X-ray diffraction study of Co3O4: transition from normal to disordered spinel Sample: RUN II, T = 1190 K Physics and Chemistry of Minerals, 1990, 17, 168-172 |
9005901 | CIF | Mg O3 Si | P b n m | 4.7787; 4.9313; 6.9083 90; 90; 90 | 162.795 | Ross, N. L.; Hazen, R. M. High-pressure crystal chemistry of MgSiO3 perovskite Sample: P = .001a GPa Physics and Chemistry of Minerals, 1990, 17, 228-237 |
9005902 | CIF | Mg O3 Si | P b n m | 4.777; 4.927; 6.89772 90; 90; 90 | 162.347 | Ross, N. L.; Hazen, R. M. High-pressure crystal chemistry of MgSiO3 perovskite Sample: P = .001b GPa Physics and Chemistry of Minerals, 1990, 17, 228-237 |
Back to the search form