COD ID | Links | Formula | Space group | Cell parameters | Cell volume | Bibliography |
---|---|---|---|---|---|---|
1526693 | CIF | Al3.84 Fe1.56 H4 Mg0.6 O14 Si2 | P -1 | 5.4744; 5.4766; 9.1505 83.53; 76.68; 60.06 | 231.335 | Koch-Mueller, M.; Kahlenberg, V.; Schmidt, C.; Wirth, R. Location of (O H) groups and oxidation processes in triclinic chloritoid Physics and Chemistry of Minerals (Germany), 2000, 27, 703-712 |
9006693 | CIF | Al4 Ca O11 Si2 | P 63/m m c | 5.4223; 5.4223; 12.7041 90; 90; 120 | 323.476 | Gautron, L.; Angel, R. J.; Miletich, R. Structural characterisation of the high-pressure phase CaAl4Si2O11 Note: Biso values altered to agree with the anisotropic values, as indicated by Ross Angel, March 2004 Physics and Chemistry of Minerals, 1999, 27, 47-51 |
9006694 | CIF | Ca O | F m -3 m | 4.815; 4.815; 4.815 90; 90; 90 | 111.632 | Fiquet, G.; Richet, P.; Montagnac, G. High-temperature thermal expansion of lime, periclase, corundum and spinel Sample: PtRh10% heating wire, T = 298 K Physics and Chemistry of Minerals, 1999, 27, 103-111 |
9006695 | CIF | Ca O | F m -3 m | 4.819; 4.819; 4.819 90; 90; 90 | 111.91 | Fiquet, G.; Richet, P.; Montagnac, G. High-temperature thermal expansion of lime, periclase, corundum and spinel Sample: PtRh10% heating wire, T = 407 K Physics and Chemistry of Minerals, 1999, 27, 103-111 |
9006696 | CIF | Ca O | F m -3 m | 4.827; 4.827; 4.827 90; 90; 90 | 112.469 | Fiquet, G.; Richet, P.; Montagnac, G. High-temperature thermal expansion of lime, periclase, corundum and spinel Sample: PtRh10% heating wire, T = 500 K Physics and Chemistry of Minerals, 1999, 27, 103-111 |
9006697 | CIF | Ca O | F m -3 m | 4.833; 4.833; 4.833 90; 90; 90 | 112.889 | Fiquet, G.; Richet, P.; Montagnac, G. High-temperature thermal expansion of lime, periclase, corundum and spinel Sample: PtRh10% heating wire, T = 585 K Physics and Chemistry of Minerals, 1999, 27, 103-111 |
9006698 | CIF | Ca O | F m -3 m | 4.841; 4.841; 4.841 90; 90; 90 | 113.45 | Fiquet, G.; Richet, P.; Montagnac, G. High-temperature thermal expansion of lime, periclase, corundum and spinel Sample: PtRh10% heating wire, T = 688 K Physics and Chemistry of Minerals, 1999, 27, 103-111 |
9006699 | CIF | Ca O | F m -3 m | 4.846; 4.846; 4.846 90; 90; 90 | 113.802 | Fiquet, G.; Richet, P.; Montagnac, G. High-temperature thermal expansion of lime, periclase, corundum and spinel Sample: PtRh10% heating wire, T = 778 K Physics and Chemistry of Minerals, 1999, 27, 103-111 |
9006700 | CIF | Ca O | F m -3 m | 4.857; 4.857; 4.857 90; 90; 90 | 114.579 | Fiquet, G.; Richet, P.; Montagnac, G. High-temperature thermal expansion of lime, periclase, corundum and spinel Sample: PtRh10% heating wire, T = 875 K Physics and Chemistry of Minerals, 1999, 27, 103-111 |
9006701 | CIF | Ca O | F m -3 m | 4.867; 4.867; 4.867 90; 90; 90 | 115.288 | Fiquet, G.; Richet, P.; Montagnac, G. High-temperature thermal expansion of lime, periclase, corundum and spinel Sample: PtRh10% heating wire, T = 1001 K Physics and Chemistry of Minerals, 1999, 27, 103-111 |
9006702 | CIF | Ca O | F m -3 m | 4.876; 4.876; 4.876 90; 90; 90 | 115.929 | Fiquet, G.; Richet, P.; Montagnac, G. High-temperature thermal expansion of lime, periclase, corundum and spinel Sample: PtRh10% heating wire, T = 1116 K Physics and Chemistry of Minerals, 1999, 27, 103-111 |
9006703 | CIF | Ca O | F m -3 m | 4.882; 4.882; 4.882 90; 90; 90 | 116.357 | Fiquet, G.; Richet, P.; Montagnac, G. High-temperature thermal expansion of lime, periclase, corundum and spinel Sample: PtRh10% heating wire, T = 1222 K Physics and Chemistry of Minerals, 1999, 27, 103-111 |
9006704 | CIF | Ca O | F m -3 m | 4.887; 4.887; 4.887 90; 90; 90 | 116.715 | Fiquet, G.; Richet, P.; Montagnac, G. High-temperature thermal expansion of lime, periclase, corundum and spinel Sample: PtRh10% heating wire, T = 1289 K Physics and Chemistry of Minerals, 1999, 27, 103-111 |
9006705 | CIF | Ca O | F m -3 m | 4.894; 4.894; 4.894 90; 90; 90 | 117.217 | Fiquet, G.; Richet, P.; Montagnac, G. High-temperature thermal expansion of lime, periclase, corundum and spinel Sample: PtRh10% heating wire, T = 1390 K Physics and Chemistry of Minerals, 1999, 27, 103-111 |
9006706 | CIF | Ca O | F m -3 m | 4.902; 4.902; 4.902 90; 90; 90 | 117.793 | Fiquet, G.; Richet, P.; Montagnac, G. High-temperature thermal expansion of lime, periclase, corundum and spinel Sample: PtRh10% heating wire, T = 1485 K Physics and Chemistry of Minerals, 1999, 27, 103-111 |
9006707 | CIF | Ca O | F m -3 m | 4.909; 4.909; 4.909 90; 90; 90 | 118.298 | Fiquet, G.; Richet, P.; Montagnac, G. High-temperature thermal expansion of lime, periclase, corundum and spinel Sample: PtRh10% heating wire, T = 1573 K Physics and Chemistry of Minerals, 1999, 27, 103-111 |
9006708 | CIF | Ca O | F m -3 m | 4.915; 4.915; 4.915 90; 90; 90 | 118.733 | Fiquet, G.; Richet, P.; Montagnac, G. High-temperature thermal expansion of lime, periclase, corundum and spinel Sample: PtRh10% heating wire, T = 1656 K Physics and Chemistry of Minerals, 1999, 27, 103-111 |
9006709 | CIF | Ca O | F m -3 m | 4.926; 4.926; 4.926 90; 90; 90 | 119.532 | Fiquet, G.; Richet, P.; Montagnac, G. High-temperature thermal expansion of lime, periclase, corundum and spinel Sample: PtRh10% heating wire, T = 1812 K Physics and Chemistry of Minerals, 1999, 27, 103-111 |
9006710 | CIF | Ca O | F m -3 m | 4.913; 4.913; 4.913 90; 90; 90 | 118.588 | Fiquet, G.; Richet, P.; Montagnac, G. High-temperature thermal expansion of lime, periclase, corundum and spinel Sample: PtRh10% heating wire, T = 1882 K Physics and Chemistry of Minerals, 1999, 27, 103-111 |
9006711 | CIF | Ca O | F m -3 m | 4.937; 4.937; 4.937 90; 90; 90 | 120.334 | Fiquet, G.; Richet, P.; Montagnac, G. High-temperature thermal expansion of lime, periclase, corundum and spinel Sample: PtRh10% heating wire, T = 1964 K Physics and Chemistry of Minerals, 1999, 27, 103-111 |